Property AA3005 C1 first hot-rolling stage, longitudinal to rolling tensile reference (CC BY experimental)
AA3005, C1 first hot-rolling stage | hot-rolled sheet from Hazelett continuous-cast strip
Density
Not listed
Not listed for this material record, condition, or selected unit system.
Thermal conductivity
Not listed
Not listed for this material record, condition, or selected unit system.
Specific heat capacity
Not listed
Not listed for this material record, condition, or selected unit system.
Young's modulus
Not listed
Not listed for this material record, condition, or selected unit system.
Shear modulus
Not listed
Not listed for this material record, condition, or selected unit system.
Poisson's ratio
Not listed
Not listed for this material record, condition, or selected unit system.
Yield strength
127.93 MPa
Tensile yield strength
Experimental Measured Screening
manufacturer-supplied AA3005 heat, C1 first hot-rolling stage, longitudinal to rolling; UNE-EN 10002-1 tensile test on an Instron 4204 at 1 mm/min crosshead speed
Tensile strength
173.8 MPa
Ultimate tensile strength
Experimental Measured Screening
manufacturer-supplied AA3005 heat, C1 first hot-rolling stage, longitudinal to rolling; UNE-EN 10002-1 tensile test on an Instron 4204 at 1 mm/min crosshead speed
Elongation at break
Not listed
Not listed for this material record, condition, or selected unit system.
Maximum service temperature
Not listed
Not listed for this material record, condition, or selected unit system.