Property AA7021 continuous-cast alloy, peak aged 124 degC for 32 h (CC BY experimental)
laboratory continuous-cast non-Cu AA7021 in the article's peak-aged condition | continuous-cast billet; machined hardness and ASTM E8 tensile specimens
Density
Not listed
Not listed for this material record, condition, or selected unit system.
Thermal conductivity
Not listed
Not listed for this material record, condition, or selected unit system.
Specific heat capacity
Not listed
Not listed for this material record, condition, or selected unit system.
Young's modulus
69.25 GPa
Young's modulus
Experimental Measured Screening
laboratory non-Cu AA7021, Al-5.8Zn-1.6Mg wt.%, fabricated by continuous casting; solution treated 470 degC for 4 h and peak aged 124 degC for 32 h; ASTM E8 tensile specimen; tensile sample count, direction and test temperature not stated
Shear modulus
Not listed
Not listed for this material record, condition, or selected unit system.
Poisson's ratio
Not listed
Not listed for this material record, condition, or selected unit system.
Yield strength
295.41 MPa
Tensile yield strength
Experimental Measured Screening
laboratory non-Cu AA7021, Al-5.8Zn-1.6Mg wt.%, fabricated by continuous casting; solution treated 470 degC for 4 h and peak aged 124 degC for 32 h; ASTM E8 tensile specimen; tensile sample count, direction and test temperature not stated
Tensile strength
438.75 MPa
Ultimate tensile strength
Experimental Measured Screening
laboratory non-Cu AA7021, Al-5.8Zn-1.6Mg wt.%, fabricated by continuous casting; solution treated 470 degC for 4 h and peak aged 124 degC for 32 h; ASTM E8 tensile specimen; tensile sample count, direction and test temperature not stated
Elongation at break
Not listed
Not listed for this material record, condition, or selected unit system.
Maximum service temperature
Not listed
Not listed for this material record, condition, or selected unit system.