Material picker
0 selected Select up to 5 materials for a readable table.
Comparison

1 materials

Property Aluminum 2014-T6 die forging (NASA historical reference)
2014-T6 die forging; NASA historical minimums | die forging or separately forged test bar
Density
2800 kg/m^3
Density
Nominal
2014 alloy at 20 degC.
Thermal conductivity
Not listed
Not listed for this material record, condition, or selected unit system.
Specific heat capacity
962.32 J/kg/K
Specific heat capacity
Nominal
At 100 degC; converted from 0.23 cal/g/degC.
Young's modulus
Not listed
Not listed for this material record, condition, or selected unit system.
Shear modulus
Not listed
Not listed for this material record, condition, or selected unit system.
Poisson's ratio
Not listed
Not listed for this material record, condition, or selected unit system.
Yield strength
379.212 MPa
Tensile yield strength
Historical Specified Minimum
T6 die forging, orientation A, maximum 4 in section; converted from 55.0 ksi.
Tensile strength
448.159 MPa
Ultimate tensile strength
Historical Specified Minimum
T6 die forging, orientation A, maximum 4 in section; converted from 65.0 ksi.
Elongation at break
Not listed
Not listed for this material record, condition, or selected unit system.
Maximum service temperature
Not listed
Not listed for this material record, condition, or selected unit system.