Materials
Compare Materials
Compare candidate materials with unit-aware values and condition metadata.
| Property |
INCONEL alloy 718 annealed and aged sheet (NASA historical reference)
Alloy 718 after 1750 degF (954 degC) anneal plus aging; historical AMS minimums | sheet, strip, and plate
|
|---|---|
| Density |
8210 kg/m^3
Density
Nominal
Aged alloy at room temperature.
|
| Thermal conductivity |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Specific heat capacity |
435.136 J/kg/K
Specific heat capacity
Nominal
Handbook alloy value converted from 0.104 cal/g/degC.
|
| Young's modulus |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Shear modulus |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Poisson's ratio |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Yield strength |
1034.214 MPa
Tensile yield strength
Historical Specified Minimum
0.2% offset, AMS 5596 sheet, strip, and plate; room temperature; converted from 150 ksi.
|
| Tensile strength |
1241.056 MPa
Ultimate tensile strength
Historical Specified Minimum
AMS 5596 sheet, strip, and plate after 1750 degF anneal plus aging; room temperature; converted from 180 ksi.
|
| Elongation at break |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Maximum service temperature |
Not listed
Not listed for this material record, condition, or selected unit system.
|