Materials
Compare Materials
Compare candidate materials with unit-aware values and condition metadata.
| Property |
AA7020 cold-rolled sheet, 1 mm (CC BY experimental)
AA7020 laboratory sheet, hot rolled at 470 degC then cold rolled to 1 mm | sheet
|
|---|---|
| Density |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Thermal conductivity |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Specific heat capacity |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Young's modulus |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Shear modulus |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Poisson's ratio |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Yield strength |
310.0 MPa
Tensile yield strength
Experimental Measured Screening
laboratory hot-rolled then cold-rolled AA7020 base metal, 1 mm sheet; tensile direction and sample statistics not stated in Table 2
|
| Tensile strength |
372.0 MPa
Ultimate tensile strength
Experimental Measured Screening
laboratory hot-rolled then cold-rolled AA7020 base metal, 1 mm sheet; tensile direction and sample statistics not stated in Table 2
|
| Elongation at break |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Maximum service temperature |