Properties
Mechanical
Property Value Unit
Tensile yield strength 310.0 MPa
Ultimate tensile strength 372.0 MPa
Elongation 14.0 %
Units
Condition
Condition
AA7020 laboratory sheet, hot rolled at 470 degC then cold rolled to 1 mm
Temper
not stated; do not infer T6
Heat treatment
hot rolled at 470 degC and subsequently cold rolled; no final age treatment stated
Product form
sheet
Thickness / diameter range
1 mm
Test direction
not stated for the Table 2 base-metal values
Processing route
laboratory hot rolling followed by cold rolling
Temperature range
Tensile-test temperature is not stated in Table 2.
Notes
Experimental base-metal values for one laboratory cold-rolled 1 mm sheet; temper and sample statistics are not stated, and the values are not EN minima.
Standards

No material standards linked.

Record status
Category
Metal
Unit system
Common SI