Materials
Compare Materials
Compare candidate materials with unit-aware values and condition metadata.
| Property |
Aluminum 7075-T652 hand forging (NASA historical reference)
7075-T652 hand forging; NASA historical minimums | hand forging
|
|---|---|
| Density |
2800 kg/m^3
Density
Nominal
7075 alloy at 20 degC; handbook specific gravity 2.80.
|
| Thermal conductivity |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Specific heat capacity |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Young's modulus |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Shear modulus |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Poisson's ratio |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Yield strength |
434.37 MPa
Tensile yield strength
Historical Specified Minimum
T652 hand forging, longitudinal, thickness <=2.000 in; converted from 63.0 ksi.
|
| Tensile strength |
510.212 MPa
Ultimate tensile strength
Historical Specified Minimum
T652 hand forging, longitudinal, thickness <=2.000 in; converted from 74.0 ksi.
|
| Elongation at break |
Not listed
Not listed for this material record, condition, or selected unit system.
|
| Maximum service temperature |
Not listed
Not listed for this material record, condition, or selected unit system.
|