Metal
Aluminum 7075-T652 hand forging (NASA historical reference)
Historical longitudinal minimum tensile properties for a thin 7075-T652 hand forging plus alloy density from the public-use NASA handbook.
Properties
Physical
| Property | Value | Unit |
|---|---|---|
| Density | 2800 | kg/m^3 |
Mechanical
| Property | Value | Unit |
|---|---|---|
| Ultimate tensile strength | 510.212 | MPa |
| Tensile yield strength | 434.37 | MPa |
| Elongation | 9 | % |
Units
Condition
- Condition
- 7075-T652 hand forging; NASA historical minimums
- Temper
- T652
- Heat treatment
- T652 precipitation heat treatment and stress relief
- Product form
- hand forging
- Thickness / diameter range
- less than or equal to 2.000 in (50.8 mm), as-forged short-transverse thickness
- Test direction
- L, longitudinal
- Processing route
- wrought aluminum hand forging
- Temperature range
- 20 ... 20 degC
- Notes
- Historical reference data transcribed with the stated property semantics and SI conversions. Confirm against the official PDF, a current procurement specification, the actual product form and thickness, and a material test report before engineering use.
Standards
No material standards linked.
Record status
- Category
- Metal
- Unit system
- Common SI