Properties
Mechanical
Property Value Unit
Hensel-Spittel coefficient A 285.0 MPa
Hensel-Spittel coefficient a1 -0.003 -
Hensel-Spittel coefficient a2 0.15 -
Hensel-Spittel coefficient a3 0.015 -
Hensel-Spittel coefficient a4 0.0 -
Hensel-Spittel coefficient a5 0.0 -
Hensel-Spittel coefficient a6 0.0 -
Hensel-Spittel coefficient a7 0.0 -
Hensel-Spittel coefficient a8 0.0 -
Units
Condition
Condition
cast EN AW-1080A as hot-compression tested
Temper
cast condition; no wrought temper applies
Heat treatment
not stated beyond the thermal cycle imposed during each compression test
Product form
cast stock; machined cylindrical compression specimen
Thickness / diameter range
10 mm specimen diameter x 15 mm length
Test direction
compression direction relative to casting geometry not stated
Processing route
cast aluminum, machined cylinder, resistance-heated Gleeble 3800 compression
Temperature range
20 ... 500 degC
Notes
The complete Hensel-Spittel coefficient set and Equation 1 convention are retained for cast EN AW-1080A over the stated hot-compression grid. A is represented in MPa and the empirical a_i values must be used together with the paper's equation and temperature convention. The article does not report replicate count, fit uncertainty or raw tabular flow curves. This is a forming-model reference, not a room-temperature tensile minimum or design allowable.
Standards

No material standards linked.

Record status
Category
Metal
Unit system
Common SI