Properties
Mechanical
Property Value Unit
Ultimate tensile strength, ST 1082.0 MPa
Tensile yield strength, ST 1054.0 MPa
Elongation, ST 4.0 %
Units
Condition
Condition
17-4PH heat 690254; H1050; 5.4 cm plate
Temper
H1050
Heat treatment
H1050 as reported; detailed schedule is not restated in Table 2
Product form
plate
Thickness / diameter range
5.4 cm (54 mm)
Test direction
ST (short transverse)
Processing route
wrought plate from identified heat 690254
Temperature range
Table 2 does not state a test temperature; no temperature extrapolation is allowed.
Notes
Measured values for one identified 17-4PH heat in 5.4 cm H1050 plate; not a thin-sheet value, population minimum, or procurement specification.
Standards

No material standards linked.

Record status
Category
Metal
Unit system
Common SI