Properties
Mechanical
Property Value Unit
Swift strength coefficient, C 539.7 MPa
Swift prestrain offset, epsilon0 0.011 -
Swift hardening exponent, p 0.2465 -
Normalized yield stress ratio, 0 deg 1.0 -
Normalized yield stress ratio, 45 deg 0.979 -
Normalized yield stress ratio, 90 deg 0.992 -
Normalized biaxial yield stress ratio 1.003 -
Lankford coefficient, RD 1.14 -
Lankford coefficient, DD 0.34 -
Lankford coefficient, TD 0.62 -
Biaxial plastic strain ratio 0.61 -
Units
Condition
Condition
AA6016-T4 alloy sheet used for anisotropic plasticity and fracture calibration
Temper
T4
Heat treatment
T4 as identified by the article; detailed prior solution/natural-ageing schedule is not stated
Product form
sheet
Thickness / diameter range
1.5 mm tensile-specimen gauge thickness
Test direction
rolling direction reference with 0, 45 and 90 deg uniaxial and biaxial ratios
Processing route
wrought sheet; detailed manufacturing route not stated
Temperature range
The source tables do not state the test temperature; no temperature extrapolation is allowed.
Notes
Reported/calibrated constitutive and anisotropy parameters for exact AA6016-T4 1.5 mm sheet. Tables 1-2 cite earlier experiments; the values are dimensionless ratios or model parameters, not absolute EN tensile minima, product allowables or a complete material card.